A216 specifies that "castings shall be furnished in the annealed, or normalized, or normalized and tempered conditions unless supplementary requirement S15 is specified." So if you are supplying A216 Gr. WCC, then as-cast is not an option anyway. Supplement S15 specifies Q&T heat treatment, so that could be an option. You might be able to meet the impacts with N&T and a low CE, but again, to agree with Metengr, it might be iffy.