dans95
Mechanical
- Jan 25, 2006
- 21
I have been assigned the task of looking into the feasibility of changing the materials of some parts which are currently made of Ultem (PEI) to Valox (PBT). Ideally we want to do this with minimal change to the tooling. Anyone have experience with these materials?