No, you cannot do that.
The welder's qualification test has nothing to do with the PQR (or WPS for that matter), unless as david stated, the welder performed the welding for the PQR qualification also.
The welder's range of thickness qualified is based solely upon the thickness of the test coupon that was used during his qualification test.