Good morning, gentlemen:
We have a WPS, due to customer request it is required to change the welding process: FCAW (E71T8) will replace SMAW (E 7018), The question is if we should make a new PQR. No impact required, Standard: ASME IX.



Thanks for your attention

JATE





 
This feels like asking the obvious. Which parts or sections of ASME IX have you reviewed so far that gave you the impression that the welding process is or isn’t an essential variable?

/edt: what’s your construction code?


Huub
 
Your qualified and experienced welding engineer will tell you.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 