I was about to condemn a strainer that was ordered as 316SS because it was magnetic and did not recognize the CF8M designation until later looking it up.
Should I condemn it anyway, as it is magnetic? Should I get it more thoroughly analyzed? Is there something in the casting process that imbues magnetic properties in 316?
Should I condemn it anyway, as it is magnetic? Should I get it more thoroughly analyzed? Is there something in the casting process that imbues magnetic properties in 316?