Other than the two hits that I get from Google, can anyone give me any more info on CF8C+?

Thanks
 
Type in "CF8C-Plus" in the Google search engine and you will get a lot more hits.
 
Article on CF8C-Plus in the October 2003 issue of the ASM Journal "Advanced Materials & Processes" which includes contacts for additional information.
 