May 24, 2006 #1 alloyhunter Aerospace Joined May 24, 2006 Messages 1 Location US how do I effectively remove all the cerrobend or utectic alloy from the inconel machined turnings so this inconel material can be recycled back into ingot for casting.
how do I effectively remove all the cerrobend or utectic alloy from the inconel machined turnings so this inconel material can be recycled back into ingot for casting.
May 26, 2006 #2 finman Mechanical Joined May 2, 2003 Messages 95 Location GB Depending upon the Cerrobend alloy you could Sieve the turnings in Hot water. Upvote 0 Downvote