While performing welds in accordance to AWS D1.1, how is ceramic backing tape categorized?
Is it seen as steel backing strip?
We have a repair project in which we will be using the ceramic as the backing, and we will be qualifying the welders with a setup as shown in Figure 4.21 (2006 Edition). I would like for the qualification to be performed with the ceramic tape in place of the steel backing. Is this allowable per D1.1?
The repair is of Carbon Steel parts, A36 material. FCAW with E71T-1 filler.
Thanks for the help.
Chris
Is it seen as steel backing strip?
We have a repair project in which we will be using the ceramic as the backing, and we will be qualifying the welders with a setup as shown in Figure 4.21 (2006 Edition). I would like for the qualification to be performed with the ceramic tape in place of the steel backing. Is this allowable per D1.1?
The repair is of Carbon Steel parts, A36 material. FCAW with E71T-1 filler.
Thanks for the help.
Chris