Hi all,
I've been given the task of figuring out how to centerless grind some of our parts in-house. It's a sleeve roughly 4" in length, .7500/.75005 12Ra finished OD, with a .4995/.5005 finished ID. They are made from 9310, with a case depth of .035/.045 and hardness of 59/61Rc, core hardness of 32/44Rc. They also have to be nital etched afterward. I'm having a difficult time finding any information on the internet or in literature. I have a limited number of setup pieces, so any advice on speeds and feeds would be helpful.
Thanks in advance!
I've been given the task of figuring out how to centerless grind some of our parts in-house. It's a sleeve roughly 4" in length, .7500/.75005 12Ra finished OD, with a .4995/.5005 finished ID. They are made from 9310, with a case depth of .035/.045 and hardness of 59/61Rc, core hardness of 32/44Rc. They also have to be nital etched afterward. I'm having a difficult time finding any information on the internet or in literature. I have a limited number of setup pieces, so any advice on speeds and feeds would be helpful.
Thanks in advance!