TConservatorSI
Chemical
I have some cellulose acetate that is degrading. It has become very brittle. I was thinking that it is from glycosidic cleavage of the polymer, but I do not know what is causing this. Also what causes plasticizers (Diethyl Phthalate and Dimethyl Phthalate and Triphenyl Phosphate to leech out? Is it the hydrolysis of the Acetate groups causing acetic acid that makes the plasticizer come out or does it just come out on its own after a certain amount of time. Is ther a certain material that will cause the plasticizer to come out faster than it normally would?