Jun 8, 2018 #1 mageshbabu12124 Materials Joined Nov 11, 2017 Messages 16 Location HK Can we bond rubber with metal after cathodic electro deposition coating?
Jun 8, 2018 #2 ornerynorsk Industrial Joined Feb 5, 2002 Messages 3,198 Location US Talk with a reputable adhesives manufacturer such as Henkel or 3M. There are adhesives for nearly everything these days. It is better to have enough ideas for some of them to be wrong, than to be always right by having no ideas at all. Upvote 0 Downvote
Talk with a reputable adhesives manufacturer such as Henkel or 3M. There are adhesives for nearly everything these days. It is better to have enough ideas for some of them to be wrong, than to be always right by having no ideas at all.
Jun 9, 2018 #3 GrahamBennett Materials Joined Feb 1, 2007 Messages 1,308 Location GB Also talk to your local Chemlok supplier. forumtowers.com Upvote 0 Downvote
Jul 10, 2018 Thread starter #4 mageshbabu12124 Materials Joined Nov 11, 2017 Messages 16 Location HK Thanks all Upvote 0 Downvote