I am having difficulty achieving a ferrite above the 35% minimum as required in NACE MRO 103. I am using E2209-16 rod and solution annealing the weld at 2150°F. The last test I did had a ferrite of 35% in the cap but only 30% in the midweld. I am restricting the interpass temperature to 300°F do I need to restrict it further?