I am trying to set up a test to rank several materials (probably a dozen or so different material samples) with regard to their ability to withstand cavitiation damage. I am looking for someone who has a flow test set up that can produce cavitation. Anybody know of a test lab or university that has test equipment in place for such testing?
 
Try with "SIET":
in Piacenza (Italy). We performed some Cv and steam test at their facilities: maybe they can help you!!
Good luck, 'NGL
 