125 kpph water tube boiler with scr (19% aqueous nh3) and co catalyst burning ulsd (15 ppm sulfur) getting white/brown (not blue) smoke at low loads (25% fire rate). Clears up at when firing rate is raised. Exceptionally long stack, 50% is horizontal, CO is zero, Nox is 9 ppm, nh3 is 4 ppm, O2 is 6%. Any ideas?
 
Replies continue below

Recommended for you

Fuel may be off spec and your not burning everything. Have you tried increasing O2?

"Scientists dream about doing great things. Engineers do them." -James Michener
 
Yes, O2 was increased and condition (opacity - white smoke) worsened.

Lowered O2 and condition got better but CO started to form (O2 is down around 3% at 100% fire with decimal CO)) Decreased nh3 injection, condition worsened. Stack temp. is around 290 F. Thanks
 
I wonder whether the following link would be helpful:

www.alentecinc.com/papers/AMMONIA/-AMMONIA_FCG.pdf
 