Dec 7, 2012 #1 arash807 Mechanical Joined Aug 8, 2012 Messages 48 Location IR Can we use cathodic protection in order to eliminate corrosion in underground galvanized piping?
Dec 10, 2012 #2 rconner Civil/Environmental Joined Mar 18, 2005 Messages 1,733 Location US While eliminate may be a strong word notice discussion at e.g. http://eng-tips.com/viewthread.cfm?qid=95745. While maybe not your application, sounds like most folks talk about coating/wrapping steel pipe with dielectric coatings when CP is envisioned. Upvote 0 Downvote
While eliminate may be a strong word notice discussion at e.g. http://eng-tips.com/viewthread.cfm?qid=95745. While maybe not your application, sounds like most folks talk about coating/wrapping steel pipe with dielectric coatings when CP is envisioned.