mojtababalaj
Petroleum
Hi everybody!
We have got a failure of four Sundyne pumps model LMV-331 (400 hp). It had an unusual pattern that we have never seen before. Bearing damage is evident on the lower input shaft in all cases. The pump had been running for about 10 days since the first start-up of the unit after overhaul. The pump tripped off on high vibration. The Input shaft bearings (Items 125C and D) are spherical roller bearings. 22310 E/C3 SKF for upper bearing and 21308 EW SKF for lower bearing are installed on low speed shaft (3000 RPM). In these failures, the lower input shaft bearings are failed dramatically. Pitting on the upper row of the rollers of the lower input shaft bearing (21308 EW) is evident. The failure is similar to surface fatigue. The pitting of the surface material is seen on the inner and outer cages of the lower bearing (21308 EW), too. It should be noted that other components of the gear box are completely healthy. Numbers of pictures of the failure are attached. the operating power of the pumps is around 240 kW.
How did you resolve this problem? Why may this failure happen?
Has anyone else experienced similar failure on the spherical roller bearings as I have described?
Regards!
We have got a failure of four Sundyne pumps model LMV-331 (400 hp). It had an unusual pattern that we have never seen before. Bearing damage is evident on the lower input shaft in all cases. The pump had been running for about 10 days since the first start-up of the unit after overhaul. The pump tripped off on high vibration. The Input shaft bearings (Items 125C and D) are spherical roller bearings. 22310 E/C3 SKF for upper bearing and 21308 EW SKF for lower bearing are installed on low speed shaft (3000 RPM). In these failures, the lower input shaft bearings are failed dramatically. Pitting on the upper row of the rollers of the lower input shaft bearing (21308 EW) is evident. The failure is similar to surface fatigue. The pitting of the surface material is seen on the inner and outer cages of the lower bearing (21308 EW), too. It should be noted that other components of the gear box are completely healthy. Numbers of pictures of the failure are attached. the operating power of the pumps is around 240 kW.
How did you resolve this problem? Why may this failure happen?
Has anyone else experienced similar failure on the spherical roller bearings as I have described?
Regards!