Hi,

I'm going to install a exhaust stack for a CAT generator set. Followings are the model data,

Gen Model- SR 4B , 1000 kva, 800 kW, 400 V, Diesel Engine
Exhaust gas flow rate – (25-30)Nm3/min
Exhaust system back pressure – 6.7 kpa

At the moment it has a 12" dia exhaust with a muffler. But the muffler is not enough to reduce noise and existing exhaust end should be changed as our requirements. Because I'm going to extend the exhaust stack and join a secondary muffler.

1.) For new stack extension 1 nos-90 and 1 nos-60 bends will be added. To reduce the back pressure effect is it ok to use 14 inch dia for new stack?

2.) I have decided to use stainless steel material. Can any one tell me the require thickness for 14" exhaust stack?

Thanks
 
You will have to design your own stack not to exceed 6.7kpa pressure. Note that exhaust is a different than air.
 