I am interested in learning more about mmc as applicable to cast wear parts used in mining industries. Much of this work is patented and not readily available. I shall be thankful,if some of the concerns that I have can be addressed
Preforming of ceramic inserts to be placed in the mold cavity.
Improving wetability between liquid steel and inserts( I assume they are honeycomb type cassettes,placed)
Anchoring of the inserts appropriately so they do not flow off or get displaced while molten metal is poured.
How to determine the size of opening for the liquid steel to flow and cover the complete mass.
Any restriction on thickness of the insert or ratio of ceramic section thickness to the section thickness of the part.
These are very direct questions related to manufacture of wear parts. However, if I can get some information or literature references, I shall be very thankful.
_____________________________________
"The richer we have become materially, the poorer we have become morally and spiritually." Martin Luther King Jr
Preforming of ceramic inserts to be placed in the mold cavity.
Improving wetability between liquid steel and inserts( I assume they are honeycomb type cassettes,placed)
Anchoring of the inserts appropriately so they do not flow off or get displaced while molten metal is poured.
How to determine the size of opening for the liquid steel to flow and cover the complete mass.
Any restriction on thickness of the insert or ratio of ceramic section thickness to the section thickness of the part.
These are very direct questions related to manufacture of wear parts. However, if I can get some information or literature references, I shall be very thankful.