An ingot rotating distributor, wheel shaped is currently made in DI (sg )ferritic iron but it is corroded by liquid zinc supposed to be transferred to ingot molds. Any suggestion for a different cast iron or alternative material? Thanks

Julio
 
Replies continue below

Recommended for you

You can try flake graphite iron instead of SG iron for the application. What material is the ingot mold? Use the same material if possible.