Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Cast CS & LTCS Gate Valves (ASTM A216 Grade WCB 600 Flange ASME B16.5 RF)

Status
Not open for further replies.

ZAbbas101054

Materials
Joined
May 18, 2014
Messages
6
Location
SA
Hi experts,

Could some one confirm if the heat number/lot number is mentioned on the subjected valves disc ? Our clint has rejected the valves at site and commented that the valves are rejected because no heat/lot number was found on the disc of gate valves.

Best Cares,
 
Take a look at ASTM A703, General Requirements for Pressure Containing Parts. Para. 17 will give you the marking requirements. Construction codes etc. can also enter into the picture. The A703 requirements (or A985 for investment cast)supersede the material specification requirements if there is a conflict.
 
Thanks sir.
Is this also applicable on seat?
 
Thread No. 408-195861 discusses pressure parts and vessels. It is worth looking at. My opinion is that the component should be traceable regardless of what the specification says, just as a way of covering yourself in the event of a problem.
 