how does a double quench and single quench method for case hardening, effect the properties of the material.
In what cases double quench is preferred?
What is the difference in microstructure expected for each case as:
1) carburising 920 for 2 hrs: 840 deg C for 45 min: oil quench
2) Carburising 920deg for 2 hrs: annealing to 600deg C:840 DEG c FOR 45 Min: oil quench
3) Carburising 920 deg Cfor 2 Hrs:Annealing to 300 deg C: 840 deg C 45 minutes: oil quench
In what cases double quench is preferred?
What is the difference in microstructure expected for each case as:
1) carburising 920 for 2 hrs: 840 deg C for 45 min: oil quench
2) Carburising 920deg for 2 hrs: annealing to 600deg C:840 DEG c FOR 45 Min: oil quench
3) Carburising 920 deg Cfor 2 Hrs:Annealing to 300 deg C: 840 deg C 45 minutes: oil quench