ataurino916
Nuclear
I need some help in the procedural process method of carburizing 400 series stainless steel material. Material is purchased in the annealed condition. Roughed out, heat treated to condition "T" or "H" as applicable per drawing requirements, machined to drawing details, carburized at shoulder bearing face per drawing (parts manufactured is a stem with acme and unified threads)and then final grinding on the diameter and bearing face. Problems arising are pitting and cracking like indications on the threads and other areas of the part. Our vendors that do this process claim they stop off all areas except the nitrided area so no other surface will be case hardened. Threads are distorting and chipping, not accepting gages after treatment. Would a 40 hour cycle be appropriate?
Threads ACME/Unified are single-pointed method machined.
Any help, in ways to manufacture?
1 part is 410 SST, other is 416 is accordance with QQ-S-763 / SAE-AMS-QQS763.