Abualnassr
Mechanical
Hi.
We have a GE blower with the following specs:
dp = 0.5 Bar
Capacity = 7060 m^3/hr
Impeller material is SS403
Speed = 5800 rpm
Suction Temp = 138 C
Discharge Temp = 208 C
Brake Horsepower = 234 HP
Gas is Chlorine
But, the process is higher than the equipment specs where capacity is actually can go up to 8700 m^3/hr and suction temperature can go up to 200 C.
Now, the main problem we are facing as maintenance department is the failure of carbon seal rings.
We use 2 carbon rings (3-segmented design) and we almost replace the rings once every 2 month.
Any ideas regarding the failure and how we can prevent it.
Best Regards,
We have a GE blower with the following specs:
dp = 0.5 Bar
Capacity = 7060 m^3/hr
Impeller material is SS403
Speed = 5800 rpm
Suction Temp = 138 C
Discharge Temp = 208 C
Brake Horsepower = 234 HP
Gas is Chlorine
But, the process is higher than the equipment specs where capacity is actually can go up to 8700 m^3/hr and suction temperature can go up to 200 C.
Now, the main problem we are facing as maintenance department is the failure of carbon seal rings.
We use 2 carbon rings (3-segmented design) and we almost replace the rings once every 2 month.
Any ideas regarding the failure and how we can prevent it.
Best Regards,