I´m working on a project for the design of a plant to produce Molecular Sieves from biomass.
I need information about their uses, production and consumption volumes, production process, etc. I know PSA is major use of CMS but I´m having hard time to find information about who uses PSA or who consumes CMS.
Please, let me know where to find information about this.
Thank you.

 
Replies continue below

Recommended for you

Do an internet search for pyrolisys. I recently did a feasibility study and got some numbers regarding the use of activated carbon (more so the cost etc)
 
PSA Nitrogen plants use CMS to remove oxygen from compressed air. Carbotech, Germany is a major manufacturer of CMS. Their website can be of some help.

Regards,
 