Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

carbon manganese or non carbon managenese material - ungroup as per ASME SEC 9

Status
Not open for further replies.

EngrRodri

Mechanical
Joined
Apr 30, 2015
Messages
37
Location
AE
Dear Experts,

Please help. why does the ASME SEC 9, in there material list with correspond to P-no (parent number) & group Number, that some materials are not listed. what is the reason why does those material are not included in ASME SEC 9 QW-422
In my case.. Im using ASTM A707 it is not included in list... so it means it is not C-MN carbon Manganese group-as per P1 material.. please enlighten
 
No. These are two reasons for not listing a specific material specification in Table QW-422;

1. There has been no request by the B&PV community to use this material for B&PV applications.
or

2. The material does not meet the ductility requirements after welding or is not readily weldable because of alloy content.
 
Thank you for feed back. Because I will do PWHT for A707 cl3 l5 . 23 mm thick Material, however in applicable code B31.8 it does not require PWHT. we had done twice our PQR however still the hardness fails. so my solution is to have PWHT.
I ask C-Mn because in B31,8 it only tells C-Mn material which i can show to client about this
 