hi!

so my previous question was whether a 1mm thickness of carbon/epoxy would be able to withstand -37psi. this is what my calculations say - i'm just wondering if it makes logical sense...those of you with more experience?

the material is carbon fiber and epoxy, diameter is 2.5in, filament winding technique.

cheers,
gyanam
 
What is the Code of Construction?
How is the pipe supported (what is the unsupported length)?

I'm a little less familiar with carbon fibre / epoxy. What is the effective compressive Young's Modulus? I know that the carbon fibres are excellent in tension, but how about compression?
 
i'm thinking of filament winding the pipe. it's about 25 centimeters in length and looks like an 'S' - so it's bent twice with two 90°s. and it's supported at the two ends.

the effective compressive young's mod is 140GPa, its tensile strength is 1500MPa and compressive is 900MPa.
 