i have an injection molding and im looking to have it made to look like carbon fibre.

are there many options to make it look like carbon fibre.
currently i have found immersion graphics as my only option??
 
Replies continue below

Recommended for you

I'm >>guessing<< you could texture the appropriate surfaces with a deep glass cloth texture, mold it in black resin or paint it black, then apply a thick coat of clear paint or resin. ... probably a lot more expensive than a layer of preprinted film.





Mike Halloran
Pembroke Pines, FL, USA
 
Does the whole part need to look like carbon fiber or just certain areas? In-mold decorating may be an option if only portions of the part need this appearance.
 
not the whole piece, i only require the front face to be carbon look.

i looked at in mold decoration and it seems to be more expensive than immersion
 
Is the part design such that a label would do the trick?
 
multiple planes, and multiple surfaces, a label would not fit.
 
Some labels can be stretched over compound curves. You should talk to someone who makes them before ruling them out.



Mike Halloran
Pembroke Pines, FL, USA
 
would stretching the label still keep true to a carbon fibre look?? ill look into it.
 
arbon fibre fabric also distorts a bit as you draw it over compound curves.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor