Dear All,

Carbon Equivalent (CE) number defines the weldability of the steel, the lower CE the better weldability,
Is there a table for CE for known steel grades? and if no why ?
There is a formula for calculation CE=C+(Mn/6)+((C+Mo+V)/5)+((Ni+Cu)/5)

If we take for example a 316L SS that is having following composition:
(C)<0.03%
(Mn): ≤ 2.00%
(Cr): 16.00 - 18.00%
(Mo): 2.00 - 3.00%
(Cu): ≤ 0.75%
(Ni): 10.00 - 14.00%

Considering the average values:
  • Cr = 17.00%
  • Mo = 2.50%
  • Cu = 0.75%
  • Ni = 12.00%

Gives for 316L CE≈5.11
However in for example "API 577 welding processes, inspection and metallurgy" paragraph 10.8.2. metallurgy and weldability (and other sources) it says steel with CE<0.35 have excellent weldability, steels with CE >0.5 poor weldability.

316L is considered a steel with an excellent weldability whereas its calculated CE turned out to be 5.11 ?
What do i miss ?
 
Replies continue below

Recommended for you

CEV is applicable to carbon and low alloy steels only. Austenitic stainless steel is a different animal. The value is an indicator of hardenability and gives a guide to the measures that may need to be instituted to reduce the likelihood of weld cracking.
 
Wrong alloy for that formula.
Weldability of austenitic alloys is evaluated differently.
 
Is there a table for CE for known steel grades? and if no why ?

The EN/ISO steel fabrication standards give for (almost) each alloy the max. CE. Carbon steel that is, not stainless steel!
As there is a range for each alloying element, there's also going to be a range for CE. Lower limit isn't of much use, so they only give the max. value.
 