Hell, in Wikipedia Carbon Equivalent Limitation for Weldability of Steels is defined as:
Carbon equivalent (CE) Weldability
Up to 0.35 Excellent
0.36–0.40 Very good
0.41–0.45 Good
0.46–0.50 Fair
Over 0.50 Poor
I looked through AWS D1.1 and AWS D1.4, but i failed to find the definition of Carbon equivalent for weldability of steel. So I want to know in which code could i find the definition for Carbon Equivalent Limitation for Weldability of Steels
Thank you!!