Carbon Equivalent Formula

Status
Not open for further replies.

Dinosaur

Structural
Mar 14, 2002
538
I recently learned that there are more than one carbon equivalent (C.E.) formulas out there. The formulas I am interested in understanding are the AWS and the ASTM versions.

The AWS version includes a term Si/6. The ASTM version includes a term V/5. Can anyone explain the difference? I noticed that ASTM A709 steels contain up to 0.40% Si (some grades even more). The Vanadium content is limited to a much smaller level, typically 0.06% for example. If the silicon content of steel is frequently higher than the limit for Vanadium, then the AWS formula appears more strict.

Is this warranted?
 
Replies continue below

Recommended for you

Preheat in D1.1 is usually determined from Table 3.2 or Annex M (A514, A517, A709, and A710). Another option is to use equations for CE in Annex XI. In Annex XI there two methods; one method based on HAZ hardness, and the other based on hydrogen control.

One draw back about using Annex XI for determining preheat is that if the preheat/interpass temp is lower than that required for prequalified WPSs, qualification testing must be performed. Ref: D1.1 Section 3.5.2
 