When i took in consideration the corrosion due to the presence of co2 in a wet stream, i was not worry because the partial pressure of co2 was inside the interval[7psi,14psi],in which "weak corrosion could occur" .And also i have 10 psi only in a KO drum and the stream is wet only when the dehydration unit is in shut-down (a very exceptional case!!!).
Taking in consideration the last case, my owner ask me to change material. Upgrading the material in my case means using SS instead CS. For avoiding this upgrade, i was looking for a epoxy coating system for a carbon dioxide corrosion in a wet system.
The use of dewaard-milliams system is only to understand if, using 3mm of corrosion allowance with CS, 20 years of lifetime of the plant could be granted. But of course, it was only an "academic" attempt, because firts of all it's everywhere underlined that this model is very conservative and then i was taking in consideration the worst case (dehydration unit in shut-down and the plant still in operation).