The carbon content in A234 WP11 and A182 F11 looks like it can either be 0.20% max or 0.15% max.
a fabricator has stated... "if the design does not dictate the need for the higher carbon content, it would be wise to select the 0.15% max since this level does not require PWHT while the .2% does"
it there a reason I would need the extra carbon. The A335 P11 pipe has a max of 0.15%.
thanks
mark
a fabricator has stated... "if the design does not dictate the need for the higher carbon content, it would be wise to select the 0.15% max since this level does not require PWHT while the .2% does"
it there a reason I would need the extra carbon. The A335 P11 pipe has a max of 0.15%.
thanks
mark