I know that carbide bands form in the process of hot forming and you have to cool the material to stop them, but it is possible that you can diminish them by simply changing the heat treatment when preparing the sample for microstructural analysis?
 
Replies continue below

Recommended for you

Good reference; the abstract pretty much describes the problem and the fix.
 