Hardening a roller might not do too much; I recall a thread ;-) where the OP was asking about something harder that steel to prevent cotton thread from cutting into rollers. thread367-92753

TTFN (ta ta for now)
I can do absolutely anything. I'm an expert! faq731-376 forum1529 Entire Forum list
 
Some boats don't have rollers. In the Navy towing manual they recommend cap rails be at least 50 HRC.
 
Thread guides are usually ceramic these days.
And it still cuts into them eventually.
I believe that the USN sometimes used PH stainless for these wear parts then they don't worry about corrosion either.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 