Dec 17, 2008 #1 jeanpaul Industrial Joined Apr 25, 2002 Messages 26 Location EU Hello Do you know a supplier of captive screw for thermoplastic? The kind without the need for an insert...
Hello Do you know a supplier of captive screw for thermoplastic? The kind without the need for an insert...
Dec 17, 2008 #2 Pud Mechanical Joined Mar 26, 2003 Messages 2,713 Location GB Do you mean any of the 7.5M hits on Google for "Screws for Plastics", or do you have something else in mind? Harry Upvote 0 Downvote
Do you mean any of the 7.5M hits on Google for "Screws for Plastics", or do you have something else in mind? Harry
Dec 17, 2008 #3 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US A screw for direct tapping into thermoplastics? PT screws are well suited. Acument is a global manufacturer that should be able to supply to you anywhere. http://www.acument.com Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora. Upvote 0 Downvote
A screw for direct tapping into thermoplastics? PT screws are well suited. Acument is a global manufacturer that should be able to supply to you anywhere. http://www.acument.com Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.