Hi,
I will study with a capillary rheometer for learning rheological properties of some polymers.But I don't know this system very well.I read some article and some books about capillary rheometer.And I didn't understand some point.
For example ,why polymers seems melt fracture properties at high shear rate?.
And I will mount a pressure transducer end of the barrel to measure pressure losses at this region.But I am not sure Where is correct point for mounting transducer.
If you deal with capillary rheometer or rheology ,could you give some information about these.
Thanks for your interest
I will study with a capillary rheometer for learning rheological properties of some polymers.But I don't know this system very well.I read some article and some books about capillary rheometer.And I didn't understand some point.
For example ,why polymers seems melt fracture properties at high shear rate?.
And I will mount a pressure transducer end of the barrel to measure pressure losses at this region.But I am not sure Where is correct point for mounting transducer.
If you deal with capillary rheometer or rheology ,could you give some information about these.
Thanks for your interest