There is a possiblity that we may need to remove incorrectly heat treated HP main steam line sections ( SA 335 P91) form a commissioned power plant and send them out for N+T, or else replace them.
Is it feasible to N+T at the site using either induction heating or a portable furnace? N+T at 1850 F, typical size is 16 " NPS with bent els, each piece may be 40 ft long?
It is beginning to look like there are a lot of plants with this issue.