I've seem to have found a denickelification on a Monel alloy (63% Ni - 31% Cu) which was in contact with HF (40% and 70% concentration). I haven't find anything about this, denickelification seems to happen in cupronickels (30% Ni and 30% Cu) but not in base Ni alloys!
Can anyone give more detail about this?
 
Replies continue below

Recommended for you

I've seen what seems to be denickelification of Monel alloy tubes in high pressure feedwater heaters in an electricity generating station. I can't tell you much more except that it is a known phenomenon even in this high-purity steam/water environment.
 