Spoonful
Mechanical
- Oct 18, 2008
- 175
Hi All,
As per ASME VIII Div 1, fig uw-16.1 type f-4 nozzle connection, it has shown as welded from both side, inside and outside, due to geometry limitation, it is not possible to weld from the inside of the shell, is it permissible to weld only from outside. just like weld shown for type f-1?
Thanks
Spoonful
As per ASME VIII Div 1, fig uw-16.1 type f-4 nozzle connection, it has shown as welded from both side, inside and outside, due to geometry limitation, it is not possible to weld from the inside of the shell, is it permissible to weld only from outside. just like weld shown for type f-1?
Thanks
Spoonful