Sep 8, 2005 #1 tte Electrical Joined Apr 30, 2004 Messages 5 Location US I have fabricated carbon fiber tubes for automotive use. I plan to use this as intake tubing. Can the tubing be ceramic coated to increase its high temperature resistance? Cheers, Roy
I have fabricated carbon fiber tubes for automotive use. I plan to use this as intake tubing. Can the tubing be ceramic coated to increase its high temperature resistance? Cheers, Roy
Sep 8, 2005 #2 unclesyd Materials Joined Aug 21, 2002 Messages 9,819 Location US These people make a number of coatings for graphite and for flexible substrates. I would contact them for additional information concerning you intended application. Since your have virtualy no flexing in application it may help. Look down the page. http://www.zypcoatings.com/ Several other people make similar coatings. Upvote 0 Downvote
These people make a number of coatings for graphite and for flexible substrates. I would contact them for additional information concerning you intended application. Since your have virtualy no flexing in application it may help. Look down the page. http://www.zypcoatings.com/ Several other people make similar coatings.
Sep 8, 2005 Thread starter #3 tte Electrical Joined Apr 30, 2004 Messages 5 Location US Thanks...I shall contact them Cheers, roy Upvote 0 Downvote