3
Can anyway advise what the difference if any is of ASTM F36a and ASTM F36j. Can find anything anywhere. They appear to give out different results in gasket materials ?
 
Replies continue below

Recommended for you

ASTM F36 is a standardized method of testing for gasket materials: the intent is to define both compressibility and recovery. There are multiple testing sequences (A thru K); which one is chosen is based primarily on the material being tested. If you need more detail, go to the ASTM Standards store at and pick up the most current (2021 edition) of the standard for $50 US.

Converting energy to motion for more than half a century
 
Thanks I will check it out.
 