Apr 15, 2016 #1 dnweld Industrial Nov 3, 2014 4 Can anyone tell me what this equipment is? http://files.engineering.com/getfile.aspx?folder=4097239b-1b19-4fba-91aa-5e72abeee00b&file=image1.JPG
Apr 15, 2016 #2 hydtools Mechanical Apr 4, 2007 3,265 A surface finish guage. Profilometer. Ted Upvote 0 Downvote
Apr 15, 2016 #3 EdStainless Materials May 20, 2004 16,306 The N values are per ISO 1302 and the numbers are in microinch. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube Upvote 0 Downvote