The heat treatment condition gives you more important information than a hardness value. I can achieve a hardness value by many methods, but a specific heat treatment "recipe" brings with it a specific strength, fracture toughness, corrosion resistance, etc. Use standards like ASTM, ISO, MIL, etc. when possible.
For hardness, please use industry standard nomenclature:
HBW - Brinell with WC indenter
HRX - Rockwell with X scale (where X can be A, B, C, etc.)
HV - Vickers
HK - Knoop