We have asked this question of API 650. Below is the response.
From: Gordon Robertson [Robertsong@api.org]
Sent: Tuesday, November 14, 2006 12:13 PM
To: John Walters
Subject: RE: API 650, Tenth Edition, Addenda 4, Paragraph 3.9.7.1 Note d.
FW: API 650, Tenth Edition, Addenda 4, Paragraph 3.9.7.1 Note d. Page 1
11/6/2007
John,
36 psf is the minimum.
Best regards,
Gordon
API
Gordon Robertson
1220 L Street NW
Washington, DC 20005
P-202-682-8190
robertsong@api.org
From: John Walters [mailto:Jwalters@ptctanks.com]
Sent: Thursday, October 26, 2006 12:09 PM
To: Gordon Robertson
Subject: FW: API 650, Tenth Edition, Addenda 4, Paragraph 3.9.7.1 Note d.
Background Section; The purpose of this inquiry is to obtain an interpretation of the standard.
Main Section;
When other factors are specified by the purchaser that are less than the factors in items a-c, is the total load on the shell to be modified by increasing H1 by the ration of 36 psf to the modified total pressure, or is 36 psf the minimum load to be
applied?
Thank You,