If Welding Parameter are as follows;
Amperage Voltage Travel Speed(mm/sec)
80~100 22~30 0.78


In order to calculate the heat input, what values are to be taken ?

1) max ampere(100), max voltage(30) and T/speed (0.78)
2) min ampere (80), min voltage (22) and T/speed (0.78)
3) ave. ampere (90), ave. Voltage (26) and T/speed (0.78)
4) others
 
Replies continue below

Recommended for you

The maximum heat input is the maximum recorded during proceure qualification. If you actually recorded 100 Amps at 30 Volts at .78 mm/min, that will be your maximum in the example given.

 