Do you know how components that don't have a direct calculation for t(required) (Appendix 2 flanges, cone shell junctures nozzles etc) are handled?
In-service Inspection of Pressure Vessels Pare RB
RE-3236 REMAINING LIFE CALCULATION
Where the corrosion rate controls the life of the pressure vessel, the remaining life shall be calculated by the following:
t (actual) - t (required)
Remaining life (years) = -----------------------------
Corrosion rate
Where,
t (actual) = thickness in inches (mm) measured at the time of inspection for the imiting section used in the determination of the t (required).
t (required) = minimum allowable thickness in inches (mm) for the limiting
section of the pressure vessel or zone. It shall be the higher of the following:
1. The calculated thickness, exclusive of the corrosion allowance, required for the pressure relieving device set pressure, static head or other loading and design temperature or
2. The minimum thick permitted by the provision of the applicable section of the original code of construction
Corrosion
Rate = inches (mm) per year of metal removal as a result of corrosion
tOriginal - tactual
_________________________
years
Leonard@thill.biz
In-service Inspection of Pressure Vessels Pare RB
RE-3236 REMAINING LIFE CALCULATION
Where the corrosion rate controls the life of the pressure vessel, the remaining life shall be calculated by the following:
t (actual) - t (required)
Remaining life (years) = -----------------------------
Corrosion rate
Where,
t (actual) = thickness in inches (mm) measured at the time of inspection for the imiting section used in the determination of the t (required).
t (required) = minimum allowable thickness in inches (mm) for the limiting
section of the pressure vessel or zone. It shall be the higher of the following:
1. The calculated thickness, exclusive of the corrosion allowance, required for the pressure relieving device set pressure, static head or other loading and design temperature or
2. The minimum thick permitted by the provision of the applicable section of the original code of construction
Corrosion
Rate = inches (mm) per year of metal removal as a result of corrosion
tOriginal - tactual
_________________________
years
Leonard@thill.biz