Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations Ron247 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Calculating Torque required for twisting a tube?

Status
Not open for further replies.

kennykmk

Industrial
Mar 9, 2012
1
Hi everyone! I was wondering if I could get some direction with calculating torsion.

I have an open ended Tube made from biomedical grade Nylon and I need to figure out how much torque I will need to apply to twist the tube. The Tube has a wall thickness of .9mm and an outside diameter of 40mm. I have physical results but would like to compare them to theoretical results. Can somebody help?

Thanks,

Kenny
 
Replies continue below

Recommended for you

Certainly not with the information supplied, and probably not in any case.

At least a type of nylon and moisture conditioning status is required to even begin to think about it.

There are quite a few very different types of nylon suitable for biomedical. Most likely are type 6.6, type 11 and type 12.

They will have up to 300% difference in flex mod depending on if they have been in water or extremely dry environment for some time prior to testing.