Hi experts

Why not mentioned the formula (Af=1940 x (Cross sectional area/minimum tensile strength) when testing tensile test of A335 material in ASME section II?
Is there are any particular reason?

Carbon pipe and API5L pipe supposed to have the above formula applied

Thanks and have a good day!!




 