when a cable gland is rusted, should i replace it?. which standards for inspecting it? thanks.
 
Replies continue below

Recommended for you

Is it rust or is it some other corrosion? If it is rust (iron or steel gland) then I think that it should be replaced under all circumstances.

Then, if it is an EMC gland, you have to choose a better quality or your equipment will be soon out of spec.

Like all installation components, the gland has a function. And therefore needs to be replaced when rusty or otherwise failing. That goes for the enclosure, too. And front door. And gaskets. And everything with a "secondary" function. Keeping these things in good order is part of the maintenance process.

Gunnar Englund
 
Steel glands? I've not come across a steel cable gland before: are you sure it is definitely a gland and not some sort of conduit or pipe fitting being used as a gland? Brass glands are pretty standard, aluminium is not uncommon, nylon is common too for non-armoured cable. If the 'gland' in question is rusting, replace it with a proper gland made from a non-rusting material suited to the environment and cable.


----------------------------------
image.php
I don't suffer from insanity. I enjoy it...
 