UNS-C84400 Red Brass should contain .02% Maximum according to many sources online.
We have received cast parts that contain too much P (.030%-.040%). What problem(s) might this cause? I am having difficulty finding specific info. on this on the internet and we do not have an expert in-house.
The only thing I have found so far is that the extra P could cause pin holes in the castings.
Any help is appreciated.